Cr,Er:YSGG – Laser Crystal – Gain Medium – Customized Products
In the Er,Cr: YSGG crystal, Cr3+ replaces the Ga3+ or Sc3+, and Y3+ is replaced by Er3+, the crystal has the advantages of large size, low optical damage, high optical quality, and low lasing threshold. Flashlamp or laser diode is often used to pump the laser crystal, 970 nm laser diode is regarded as the first choice to realize 2790 nm laser pumping of Er,Cr: YSGG, which can excite the Er3+ to his lasing upper level directly with high efficiency and low energy cost. Nowadays, various method have been adopted to switch Q (such as acousto-optic, electro-optic, FTIR) to realize pulse laser output. Owing to the specificity of lasing wavelength, this kind of lasers are widely used in medical applications, scientific investigations, material processing, military and so on.
Note:
$100 is a deposit, not the final price of the product. Please contact us for price if needed.
Features
Good crystal quality
Super mechanical properties
Low pump threshold
High slope efficiency
Working at medium frequency
Material Specifications
| Crystal Structure | Cubic |
| Chemical Formula | Y2.93Sc1.43Ga3.64O12 |
| Lattice Constant | 12.42 Å |
| Concentration | 30 at % (3.7 x 1021 cm<-3 , dodecahedron Er3+) |
| 2 at % (1.7 x 1020 cm-3 , octahedral Cr3+) | |
| Wavefront Distortion(Rod length per inch) | 2-Jan |
| Surface Finish | 10–5 S–D |
| Perpendicularity | 5‘ |
| Parallelism | 30“ |
| Precise Finish | 55 microinch ± 5 microinch |
| Chamfer | 45 deg ±5 deg |
| Length Tolerance | +0.040 / -0.000 in |
| Diameter Tolerance | +0.0000 / -0.0020 in |
Physical and Chemical Properties
| Thermal Conductivity(W / mK) | 8 |
| Thermal Coefficient of Expansion | 8.1×10-6/K |
| Thermal-optical Coefficient(dn / dT)(10-6/ K) | 12.3 |
| Mohs Hardness | 8 |
| Density | 5.67g/cm3(Cr&Er doping) |
| Size(DxL),mm | From 3 x 30 to 12.7 x 127.0 |
| Orientation | <001>, <111> |
Optical and Spectral Properties
| Refractive Index | 1.92 at 1000 nm |
| Fluorescence Lifetime | 1400 μs |
| Emission Cross-section | 5.2 x 10-21 cm2 |
| Laser Wavelength | 2.791 µm |
3×1 Pump Combiner Low Insertion Loss Optical Fiber Combiner
BBO - Electro-optic Crystal - Customized Products
BGO (Bismuth germanate) - Electro-optic Crystal - Customized Products
Er:YAG Crystals (Erbium-doped yttrium aluminum garnet crystal) - Laser Crystal - Gain Medium - Customized products
CLBO (Cesium Lithium Borate CsLiB6O10) - Laser Crystal - Nonlinear Crystal - Customized Products
RTP (Rubidium titanyl phosphate) - Laser Crystal - Nonlinear Crystal - Customized Products
Fe: ZnSe(Iron-doped ZnSe) - Laser Crystal - Gain Medium - Customized products
AgGaS2(Silver Gallium Sulfide) - Laser Crystal - Nonlinear Crystal - Customized Products
Cr:BeAlO2 - Laser Crystal - Gain Medium - Customized products
2x1 Pump Combiner Optical Fiber Combiner Customized Product
Nd:YVO4 (Nd-doped yttrium vanadate) - Laser Crystal - Customized products
Yb:YAG - Laser Crystal - Gain Medium - Customized Products
Nd: YAG (Neodymium-doped Yttrium Aluminium Garnet)- Laser Crystal - Customized products
Cr: ZnSe(Chromium Zinc Selenide) - Laser Crystal - Gain Medium - Customized products
KTiOAsO4 KTA (Potassium titanyl arsenate) - Laser Crystal - Nonlinear Crystal - Customized Products
Yb:CALGO - Laser Crystal - Gain Medium - Customized products 